Complete Process for Multimetal CR STEEL, GALVANIZED STEEL Suitable for Spraying

Process

Proposed

Products

Concentration

%

Time

(min)

Temperature

(°C)

Remarks

Alkaline

Cleaning

FerroClean LF

or

FerroClean D

1-2

1-2

1-3

1-3

40-70

40-70

 

Rinse

 

 

 

 

 

Phosphating

OR

Iron S

1-2

1-3

40-60

 

ZPII

Zinc Phosphate

5-10

2-6

55-70

Heavy coating use outdoors

Nano Ceramic Coating

M Coat

0.5

0.5-1.5

28-32

 

Rinse

 

 

 

 

 

Dl Rinse

Dl water

 

 

 

 

Dry Oven

 

 

 

>100